Solid Formation
De-stabilization of a silicate solution leads to the emergence of solid particles within a liquid medium. This silica precipitation occurs when the acidity of the bath increases or when the concentration of dissolved solids exceeds the solubility limit. The resulting white particles can settle on fabric or clog the machinery in a wet processing plant.
Chemical Driver
Neutralizing a highly alkaline silicate stabilizer with acid causes the immediate formation of insoluble minerals. During bleaching, silica precipitation must be avoided to prevent the buildup of harsh scale on the surface of the stainless steel rollers. These deposits are difficult to remove and can cause physical damage to delicate fabrics.
The addition of sequestering agents helps to keep the minerals in a soluble state.
Quality Impact
Hard white spots on the dyed cloth are often the result of mineral solids getting trapped in the fibre matrix. When silica precipitation happens inside the yarn, the fabric becomes stiff and loses its natural drape. These particles also act as abrasives that wear down the needles during the sewing process.
Process Control
Managing the bath ph and the rinse water quality is the primary way to stop the formation of these solids. Regular cleaning of the peroxide bleaching range prevents the accumulation of scale that triggers further silica precipitation. Monitoring the turbidity of the liquor provides an early warning of an impending stability failure.