Hysteresis Equilibrium
Equilibrium moisture absorption in regenerated cellulose fibers after initial drying and re-exposure to specific atmospheric conditions determines the commercial mass of the material. Secondary viscose regain measures the moisture content of viscose fibers during subsequent processing stages under standard laboratory conditions. This measurement accounts for the historical drying path, since the moisture sorption of cellulosic fibers exhibits hysteresis behavior depending on whether they are wetting or drying.
It represents the actual water uptake a spinner can expect during open-air storage and drafting in the mill.
Moisture Behavior
Fibre conditioning is required because the secondary viscose regain differs from the primary regain measured immediately after fiber extrusion and first-time drying. The physical structure of the cellulose undergoes irreversible changes during the first drying cycle, which permanently reduces its water-holding capacity. Knowing this difference is crucial for mills when calculating yarn yields from raw fiber shipments.
Processing Impact
Spinning operations are highly sensitive to moisture levels because dry viscose generates static electricity during carding and drafting. If the regain is too low, fibers repel each other and stick to the metal rollers of the drafting system. Maintaining the correct moisture content in the spinning room ensures smooth processing and uniform yarn density.
Quality Verification
Commercial transactions of viscose yarn packages use these regain percentages to adjust the invoiced weight to a standardized moisture level. Standard testing labs measure the bone-dry weight of yarn samples and apply the standardized regain factor. This financial calculation prevents dispute between yarn mills and garment manufacturers.