Mechanical Degradation
Reduction in fibre length and tensile strength occurs when recycled textile materials are shredded through spiked rollers to be returned to a fibrous state. Excess garnetting damage typically results from high cylinder speeds or blunt teeth during the mechanical tearing of wool rags. This process shears the scales of the wool and creates short fragments known as flocks.
Fibre Integrity
Microscopic evaluation of the resulting shoddy often shows fractured ends. Excessive garnetting damage compromises the spinning limit, making it difficult to produce fine yarns. Shortened fibres lack the necessary overlap to maintain yarn cohesion.
Processing Limit
Mills control the extent of this destruction by adjusting the feed rate and the moisture content of the input rags. While some garnetting damage is unavoidable in the recovery of hard-woven scraps, lubricating the cloth before shredding reduces the heat and friction. High moisture levels help the fibres slide past the metal teeth rather than snapping.
Inspection Standard
Quality control teams measure the percentage of fibres below 25 millimetres to assess the severity of the opening process. When garnetting damage exceeds certain thresholds, the material must be blended with virgin fibres to meet strength requirements. The presence of excessive dust and short bits indicates a poorly maintained garnetting machine.