Extension Property
Proportion of length increase measured when a fabric specimen is pulled to the point of rupture at a constant rate of extension belongs to the category of ultimate mechanical limits. Calculating iso 13934-1 dynamic strain requires specific specimen dimensions.
Testing Protocol
Strip tests use five specimens in the warp direction and five in the weft direction to ensure a statistical average. The machine moves at a speed of one hundred millimetres per minute. Results from this method allow mills to compare the ductility of different batches of finished goods.
Production Quality
Finished fabrics must meet the minimum elongation requirements specified in the purchase contract to withstand garment assembly. While static strength is important, iso 13934-1 dynamic strain provides a clearer picture of how the fabric handles sudden loads. Low values suggest a brittle fabric that might tear during wear.
Technical specifications for outdoor gear often mandate a higher percentage of extension to account for environmental stresses.
Load Curve
Data collected during the test shows the relationship between the applied force and the resulting deformation. A steep curve indicates a stiff material with low elasticity. Analysis of the break point confirms if the fabric meets the industrial standard for its intended use.