Molecular Breakdown
Thermal hydrolytic reactions break the polymer chains of polyester during the melt spinning process. This structural damage causes intrinsic viscosity degradation and reduces the molecular weight of the recycled resin. The material becomes more fluid and loses its structural integrity.
Spinners monitor the melt flow index to detect this degradation.
Extrusion Stress
High temperatures and residual moisture in the extruder barrel accelerate the cleaving of ester linkages. Moisture levels above fifty parts per million trigger rapid intrinsic viscosity degradation during the melting phase. Screw shear and residence time also influence the rate of polymer breakdown.
Dry air dehumidification before extrusion is required to maintain the stability of recycled polyester flakes.
Tensile Consequence
Low molecular weight polyester results in weak filament yarn with high break rates during downstream drawing and texturizing. Severe intrinsic viscosity degradation leads to brittle fibers that cannot withstand high-speed processing. The resulting fabric exhibits poor tensile and tear strength.
Mills must reject yarn lots that fail to meet the required viscosity threshold.
Prevention Protocol
Desiccant dryers lower the moisture content of the polymer chips to a critical threshold before they enter the spinning line. This step prevents intrinsic viscosity degradation by eliminating the water molecules that would otherwise drive the hydrolytic reaction. Vacuum solid-state polymerization can also rebuild the chain lengths of recycled polymers before melt extrusion.
Quality control laboratories test the viscosity of both the incoming raw chips and the finished extruded yarn to confirm that the protective drying process has worked effectively during the production run.