Repellency Metric
A comparative assessment score quantifying the resistance of textile surfaces to wetting by dynamic water droplets defines the standard metric for water-repellent finishing performance. Established by international testing protocols, spray rating measures macroscopic fluid shedding under controlled gravitational impact rather than pressurized hydrostatics. A specified volume of distilled water pours through an calibrated spray nozzle suspended above an inclined textile test specimen.
Visual examination of the wetting, spotting, or coating along yarn surfaces yields an integer value matched to a standardised reference chart. The metric ceases to apply to waterproof barrier testing, air permeability limits or hydrostatic head water-column determinations.
Apparatus Geometry
Testing equipment follows strict structural configurations outlined in AATCC Test Method 22 and ISO 4920 standards. A glass funnel holds exactly two hundred fifty millilitres of distilled water, discharging through a perforated spray head featuring nineteen holes of precise diameter. Liquid free-falls through a vertical distance of one hundred fifty millimetres onto the fabric specimen.
The textile sample sits mounted over a six-inch embroidery hoop positioned at a fixed angle of forty-five degrees relative to the stream. This forty-five-degree tilt prevents standing water accumulation, driving unabsorbed droplets to roll down the test plane under standard atmospheric gravity.
Grading Spectrum
Surface wetting conditions map directly to an incremental performance scale. A rating of one hundred indicates complete absence of water sticking or wetting across the sprayed face. A score of ninety registers slight random sticking or spotting on exposed fabric crowns.
An eighty rating reflects partial wetting occurring at yarn intersections. Ratings drop to seventy for complete face wetting and fifty for wetting across the entire top surface, plunging down to zero when complete water penetration drenches both face and back. Two identical test specimens must receive independent sprays, followed by quick mechanical tapping to clear unattached hanging droplets before final comparison against standard reference photographs.
Production Verification
Textile mills run spray evaluations as an operational checkpoint immediately downstream of the stenter curing process. Insufficient cure temperatures, surfactant residues in the chemical pad bath, or apex starvation consistently yield ratings below commercial purchase requirements. Workwear and technical outerwear specifications demand an initial rating of one hundred on factory-fresh cloth, dropping no lower than eighty after ten to twenty domestic wash-dry cycles.
Testing laboratories repeat the protocol on abraded samples to confirm whether repellency survives active wear. Chemical suppliers adjust fluorochemical or non-fluorinated polymer active solids based on these numerical spray values to balance formula cost against required field performance.