Polymer Application
Sizing processes apply protective polymers to warp yarns to increase their tensile strength and abrasion resistance during high-speed weaving. The warp sizing add-on is the weight percentage of size dry solids deposited on the yarn relative to the dry weight of the unsized yarn. This protective coating prevents yarn breakages caused by the heavy friction and mechanical stress exerted by the loom components.
The dry sizing film must be washed off before dyeing and finishing.
Process Control
Squeeze roll pressure and size box temperature must be kept constant to maintain uniform chemical pick-up across the entire yarn sheet. Achieving the correct warp sizing add-on involves balancing the concentration of the starch or polyvinyl alcohol solution with the speed of the sizing machine. If the add-on is too low, the yarn remains hairy and weak, leading to frequent loom stoppages and fabric defects.
Conversely, an excessive add-on makes the yarn stiff and brittle, which increases warp breakages during weaving. Technicians test the pickup level at the exit of the sizing machine.
Desizing Efficiency
Enzymatic or hot-wash treatments must remove the protective sizing agent before dyeing to ensure uniform color absorbency. The level of the warp sizing add-on directly determines the complexity of the desizing stage, since higher concentrations of starch require longer dwell times or more intensive enzyme treatments to clear the fibres. If residual size remains on the fabric, it acts as a barrier to dye molecules, causing blotchy and uneven coloration.
This chemical check is performed at the preparation checkpoint before dyeing begins.
Commercial Measurement
Standard wash-out tests on yarn samples quantify the amount of dry size solids added during the process. The mill compares the dry mass of a warp sample before and after a laboratory wash to calculate the warp sizing add-on percentage. This lab test verifies that the batch is ready for the loom.