Thermal setting over 190°C and jet nozzle pressures above 0.30 MPa degrade polyurethane cores, causing permanent set and elasticity loss in synthetic knits.

Thermal setting over 190°C and jet nozzle pressures above 0.30 MPa degrade polyurethane cores, causing permanent set and elasticity loss in synthetic knits.

Polyether elastane core retention under high shear jet dyeing requires maintaining bath pH between 5.5 and 6.0 while capping nozzle pump pressures below 1.5 bar.

High temperature jet processing of aged elastomeric fabrics induces thermal hydrolytic cleavage, reducing retractive force and causing severe roll scrap.